Key advantages
- Excellent corrosion resistance
- Low elastic modulus
- Biocompatibility
- High strength
- Fatigue resistance
Chemical composition
| Grade | Ti | Al | V | Fe | C | N | H | O |
|---|---|---|---|---|---|---|---|---|
| Ti-6Al-4V ELI | Balance | 5.5–6.5 | 3.5–4.5 | 0.25 | 0.08 | 0.05 | 0.012 | 0.13 |
| Grade 5 | Balance | 5.5–6.75 | 3.5–4.5 | 0.30 | 0.08 | 0.05 | 0.015 | 0.20 |
Mechanical properties
| Grade | Condition | Tensile Rm (MPa) | Yield Rp0.2 (MPa) | Elongation A (%) | Reduction Z (%) |
|---|---|---|---|---|---|
| Ti-6Al-4V ELI | Annealed (M) | 860 | 795 | 10 | 25 |
| Grade 5 | Annealed (M) | 860 | 780 | 10 | — |